Grinding speed-grinding time interaction was the next significant variable.These results were expected because lower grinding speed and longer grinding time generates a similar amount of grinding action compared to higher speeds and lower times.The cordierite mixture was completely amorphized by grinding at 300 rpm for 60 minutes.